Foshan Xingzhongda Industry Commerce Co., Ltd.
Products
Contact Us
  • Contact Person : Mr. DU Nick
  • Company Name : Foshan Xingzhongda Industry Commerce Co., Ltd.
  • Tel : 86-0757-85438329
  • Fax : 86-0757-85437102
  • Address : Guangdong,foshan,Xing Zhong Da Industrial Park, Luohang, Jinsha, Danzao Town, Nanhai District
  • Country/Region : China
  • Zip : 528223

Black Nickel Free Cobalt Tin

Black Nickel Free Cobalt Tin
Product Detailed
Related Categories:Other Chemicals
nickel free black nickel electroplating Plating 1, High stability 2, 5 times efficiency 3, Best price

737 nickel-free black nickel electroplating Plating  chemical

737 nickel-free black nickel electroplating Plating  chemicaltechnology is a nickel-free, nontoxic,tin-cobalt alloy electroplating processing. The coating’s color of this process can be black and bright. It’s good hardness and easily controlled color and stable plating bath made this technology suitable for every kind of black decorative electroplating.

2,Process features

a,Special beautiful black coating, the color can be selected from light black to deep black..

b,Stable electroplating bath ,wide range of technology, also stable coating color.

c,High coverage capacity, especial for barrel electroplating

d,Don’t need wastewater treatment.

e,Can be plated on bright copper ,white-colored copper/tin alloys,brass

3,Equipment

Coating bath: rigid PVC or steel bath covered by plastic.

Heating : titanium or quartz electric pen.(You’d better use the water bath to heat uniformly)

Anode : carbon board

Anode bags: needed

Mixing: cathode rocking, at least 1~2 meters in one minute or liquid flow. Using the air in stirring is not allowed.

Filtering: continuous filtering.

Barrel plating: regular semi-auto portal line, its conductive should be good, or the walk position will be difficult.

4,Operation condition

                                     Optimal      Range

Electroplating cathode current density    A/dm2    0.8       0.2~1.2

Temperature                         °C       40       35~50

Rack plating time                   second     45        30~120

Barrel plating time                  minute     10        3~30

PH                                          9        .8.5~10

Percentage                         Be°      24        22~30

Anode                                   carbon board   

Ratio: anode vs cathode                        1:1~1:2

Mixing                               cathode rocking

Black Nickel Free Cobalt Tin



Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.